KISE Journal of Korean Institute of Surface Engineering 2007;40(6):271-278. Published online: Nov, 30, -0001
DOI : 10.5695/JKISE.2007.40.6.271
In this study, applicable possibility in chemical decontamination for reactor coolant pump(RCP) was investigated for the various stainless steels. The stainless steel(STS) 304 showed the best electrochemical properties for corrosion current density and th
Keywords Reactor coolant pump;Chemical decontamination;Corrosion current density;Stainless steel;