KISE Journal of Korean Institute of Surface Engineering 2008;41(6):255-263. Published online: Nov, 30, -0001
DOI : 10.5695/JKISE.2008.41.6.255
Generally, deposition mechanism of diamond particle is mainly embedding effect in the kinetic spray process. Accordingly, in spite of high cost, helium gas was employed as process gas to get high diamond fraction in the composite coating. In this study, t
Keywords Ni coated diamond;Bronze/diamond composite;Kinetic spraying;Particle flight velocity and plastic deformation;