KISE Journal of Korean Institute of Surface Engineering 2014;47(1):33-38. Published online: Nov, 30, -0001
DOI : 10.5695/JKISE.2014.47.1.033
Nanoindentater tests were conducted to conducted nanoindentation microhardness of the individual phase of ferrite and martensite of 680MPa dual-phase (DP) steel charged with hydrogen. Hydrogen was charged by electrochemical method with current densities o
Keywords Nanoindentatier test;Electrochemical method;680MPa DP steel;Hydrogen embrittlement;