- Past Issues
- e-Submission
-
2021 Impact Factor 1.766
5-Year Impact Factor 1.674
Editorial Office
- +82-2-563-0935
- +82-2-558-2230
- submission@kssse.or.kr
- https://www.kssse.or.kr/
2021 Impact Factor 1.766
5-Year Impact Factor 1.674
KISE Journal of Korean Institute of Surface Engineering 2020;53(2):80-86. Published online: Nov, 30, -0001
DOI : 10.5695/JKISE.2020.53.2.80
This paper is concerned with type of imperfections present within the anodic oxide films on AA2024 and surface hardness of the anodic film measured after ink-impregnation. The anodic oxide films were formed for 25 min at 40 mA/㎠ and 15±0.5
Keywords Surface hardness;anodic oxide film;AA2024;ink-impregnation method;