KISE Journal of Korean Institute of Surface Engineering 1997;30(3):191-201. Published online: Nov, 30, -0001
Non-passivated electrolytic tinplates withour conventinal chemical treatment self-oxidize in ambient atmosphere to from yellow stain on the outermost surface during the long-term storage. The degree of yellowness of the stain increased linerly with the ox
Keywords Electrolytic Tinplate;Drawing and Ironing;Tin Oxide Layer;Friction Coefficient;