KISE Journal of Korean Institute of Surface Engineering 1997;30(5):320-332. Published online: Nov, 30, -0001
The development of colored surface on zinc coating by the oxidation of a melten alloy of zinc with a minor amount of oxygen-avid additive such as tianium has been studied. Using a galvanizing Zinc alloy containing 0.1 to 0.3wt%Ti, gold, purple or blue col